Lead brass
Lead is practically insoluble in brass, and distributed on grain boundaries in the form of free particles. Lead brass can be divided into α and (α+β) according to its structure. Alpha lead brass can only be cold deformed or hot extruded because of the harmful effect of lead and low plasticity at high temperature. (α+β) lead brass has good plasticity at high temperature and can be forged.
tin brass
Adding tin to brass can obviously improve the heat resistance of alloy, especially the ability of resisting seawater corrosion, so tin brass is called "navy brass".
Tin can be dissolved in copper-based solid solution, which plays a role of solid solution strengthening. However, with the increase of tin content, brittle R phase (CuZnSn compound) will appear in the alloy, which is not conducive to the plastic deformation of the alloy, so the tin content of tin brass is generally in the range of 0.5% ~ 1.5%.
Commonly used tin brass are HSn70-1, HSn62-1, HSn60-1, etc. The former is alpha alloy, which has high plasticity and can be processed by cold and hot pressing. The alloys of the latter two grades have (α+β) two-phase structure, and a small amount of R phase often appears. Their plasticity at room temperature is not high, and they can only deform in hot state.
manganese brass
Manganese has great solubility in solid brass. Adding 1% ~ 4% manganese to brass can significantly improve the strength and corrosion resistance of the alloy without reducing its plasticity.